Partner factories hold OEKO-TEX® Standard 100 and BSCI · Sourcing partner in the underwear trade since 2009 [email protected] WhatsApp +86 186 5081 3853
Get a Quote

A logo that looks right on a strike-off and looks tired on the shop floor eight weeks later is not a printing problem. It is a specification problem: the decoration method was chosen from the artwork before anyone wrote down the fibre, the exposure and the test that would settle the argument. Beach shorts are the hardest place to skip that step, because one garment is asked to survive chlorinated water, salt water, sun, abrasion against sand and a 40 °C wash cycle, and each of those attacks a different part of a decorated surface.

This page is the decision path we use for logos on beach shorts, board shorts and swim shorts: which method fits which fibre, why a print cracks while a sublimated mark fades away, what has to be in the artwork file, and the test list that belongs on the purchase order before bulk. Fabric behaviour sits in the quick-dry fabric guide; the category split is in beach shorts versus board shorts versus swim trunks; the defect side is in the beach shorts inspection checklist; the compliance frame is in the beach shorts compliance guide; and the category starting point is the beach shorts OEM page.

Xiamen Unitex Trade Co., Ltd. is a sourcing and trading company, in the trade since 2009 and incorporated in Xiamen in 2013. We are the supplier named on the purchase order, and the garments are cut, sewn and decorated by partner factories — the manufacturers audited under amfori BSCI and certified to OEKO-TEX® STANDARD 100. That structure matters here because decoration is where responsibility is easiest to lose: the buyer approves a logo, the printer approves a screen, and nobody owns the test report. Naming the party that signs the purchase order is the first control, not a formality.

Which logo method survives a beach short?

Five methods cover almost every beach short logo, and the choice is made by fibre chemistry rather than by taste. Sublimation needs polyester, because only polyester takes disperse dye into the fibre. Screen print and silicone transfer sit on top of whatever the surface is, so they work on nylon, polyester and blends, provided the ink’s elongation matches the fabric’s. Embroidery threads through the cloth, so it works on stable wovens and fights anything with elastane. Woven labels and jacquard elastic avoid the question by building the mark into a component instead of onto a surface.

Decoration methods for beach shorts, what each one does to the surface, and how it fails — Xiamen Unitex Trade Co., Ltd.
Method What it bonds to What it adds How it fails in use Where it belongs
Sublimation Polyester, 65% or more. Not cotton; weak on nylon Nothing on the surface: the dye sits inside the fibre, hand unchanged Colour leaves; the mark becomes a ghost after chlorine and sun All-over and placement prints on polyester shells
Screen print, plastisol Nylon, polyester, blends, with a cured film 80 – 150 g/m² locally; a visible film that softens after washing Cracks along the edge when the fabric extends further than the ink; peels off a water-repellent finish Chest, leg and back placement on woven shells
Screen print, water-based Cotton-rich and polyester Thin matte film, almost no hand Low colour yield on dark nylon without a base layer, which means two passes Large flat areas where hand matters
Silicone transfer Nylon, polyester, elastane blends 250 – 400 g/m²; raised, rubbery, opaque Edge lifts if the panel is stretched during pressing; blocks airflow over mesh Bold marks on stretch swim shells, panels next to the waistband
Heat-transfer film Polyester, nylon; not on a fresh water-repellent finish Thin film with a sharp edge and a slight gloss Edge lift after repeated chlorine; a gloss ring if the press runs too hot Names and numbers, small runs, short-life fashion
Embroidery Stable wovens from about 120 g/m²; fights elastane Raised thread, well under 1 g per 60 mm mark Puckers on stretch; needle holes open on coated shells; fills in below 5 mm cap height Leg hem, back pocket, heavier taslan shorts
Woven label, sewn Any shell Edges stand proud of the surface Scratches if the tape edge is cut rather than folded Centre back, side seam, waistband
Jacquard-woven elastic None — it is the elastic Nothing; the mark is yarn Limited by the weaving repeat and by the yarn colours available Waistband, when the elastic is already custom
Metal engraving Hardware: aglets, eyelets, cord ends Nothing on fabric Plating wears through to base metal in chlorinated water Drawcord ends, eyelets, cord locks
Add-on weights are typical values for a 60 mm mark, not figures from a standard. Bonding and failure follow fibre chemistry and cure temperature; cure windows are process data, and the ink supplier’s technical data sheet governs over a table. The remaining numbers on this page are trade ranges and process data, not specification limits; where a standard number appears, the standard governs.

Two rules make the table usable. First, the shell and the waistband are usually different materials, so one range can need two processes for one logo: a sublimated mark on the leg shell and a jacquard or printed mark on the elastic. Second, a method that is correct on a flat panel can be wrong at a seam, because a print pressed across a step thins the film exactly where the garment flexes most.

Close-up of a navy beach short waistband with a logo jacquard-woven into the elastic, the white yarns interlaced with the navy so the mark is flush, and the same mark showing mirrored on the reverse side
A jacquard-woven waistband mark on a navy beach short: the white yarns are interlaced with the navy while the tape is woven, so the logo is flush with the elastic and appears mirrored on the reverse. Nothing is applied or stitched on, so there is no edge to lift — the trade-off is that the design is limited by the weaving repeat and the yarn colours.

Why does a printed logo crack while a sublimated one disappears?

They are two different structures, and they fail in opposite directions. In sublimation the printed paper is pressed at roughly 180 – 200 °C, the disperse dye turns to gas, diffuses into the polyester and is trapped there when the fibre cools. Nothing is added to the surface, so there is no film to crack; the failure is colour loss, and it usually shows as a pale ghost of the original mark by the time the garment has seen a season of chlorine and sun. A screen print leaves a cured film 20 – 60 µm thick sitting on the weave. That film has its own elongation, and when the fabric extends further than the film can follow, the film gives.

The numbers explain most complaints. A four-way stretch swim shell can extend 80 – 120% across the hip. A fully cured plastisol film may stretch 150 – 200% before it breaks, which sounds like enough — but a film cured at 140 °C instead of 150 – 160 °C looks identical on the sample and fails at the first real extension. That is why the cure temperature belongs in the decoration specification and not only in the printer’s head.

Sublimation also cannot be carried across colourways without thinking. Disperse dye has low affinity for polyamide, so the same artwork printed on a nylon shell looks strong out of the press and washes grey within a few cycles; nylon is dyed with acid dyes at yarn stage, or decorated with a print film. A quotation that says the logo will be done “the same way on both colourways” is telling you that one of the two is going to be wrong in month two.

Elastane sets the temperature ceiling. Above roughly 175 – 180 °C elastane loses strength and yellows, so a calendar running at 195 °C over a shell with 18% elastane is a fabric problem before it is a print problem. On those shells the order is: print film or silicone, not sublimation; and if sublimation is unavoidable, the elastane has to be in a panel the press never touches.

Can you embroider a swim short, and where does it fail?

Every stitch is a needle perforation. On a tight woven taslan the fibres close around the thread and the holes disappear; on a laminated or coated shell the holes stay open, and the film starts to delaminate along the stitch line. The first question to ask about any embroidered swim short is therefore not how the front looks but what the reverse side looks like after two washes.

Geometry has hard minimums. A letter needs 5 mm of cap height, a satin column needs 1.2 mm of width, and two colours need 0.4 mm of gap between them, otherwise the fills merge into a blob. Those are digitising limits used across the trade rather than values from a standard — ISO 4915 governs stitch type, not minimum letter size — but a digitised file that ignores them will not sew. Below those numbers the artwork is not embroiderable and should become a woven label. On four-way stretch, embroidery needs a water-soluble stabiliser of 25 – 40 µm and a low-density underlay, and the film has to be washed out afterwards; leave it in and the panel stiffens and shows a ring after the second wash.

Placement carries the rest of the risk. Keep embroidery 15 mm clear of the waistband tunnel edge and off every bartack: a stitch line running across an elastic tunnel locks the stretch, and the wearer feels it at the waist within an hour. Weight is rarely the issue — a 60 mm mark at about 4,000 stitches adds well under a gram of 40s thread — the stiffness is. Where a seam is involved, the construction follows ISO 4915: a type 301 lockstitch for the seam and 304 zigzag at an edge tack. The embroidered mark itself is built from running, satin and fill stitches, which ISO 4915 does not classify.

Where embroidery wins is on heavier woven shells: taslan and ripstop from about 120 g/m² up, at the leg hem or on a back pocket, in markets where embroidery is read as a quality signal rather than as decoration. Where it loses is on mesh linings, coated shells, and anything that has to stretch.

How should a logo be tested before bulk?

Four attacks matter, and each one needs its own specimen: laundering, chlorinated water, light, and abrasion. They are separate tests because they destroy colour by different mechanisms, and a mark that passes one can fail the next. The table is the list we put in front of a buyer when the logo is approved.

Logo and colour-fastness tests for beach shorts, with the condition that decides the result — Xiamen Unitex Trade Co., Ltd.
Test Standard Condition that matters What a failure looks like Who sets the pass level
Colour change after laundering ISO 105-C06 The letter: S is close to one home wash, M approximates up to five washes at 70 °C or below Fading, bleeding into a white panel Brand writes the grade; typically 4
Chlorinated water ISO 105-E03 50 mg/l and 100 mg/l are the swimwear conditions; 20 mg/l describes accessories such as beach robes and towels Fading, yellowing, a hard hand Brand writes the grade
Sea water ISO 105-E02 Immersion, then drying, without rinsing Fading confined to the immersed area Brand writes the grade
Perspiration ISO 105-E04 Acid and alkaline solutions, both required Fading, staining of the adjacent panel Brand writes the grade
Rubbing ISO 105-X12 Dry and wet crock, separately Ink transferring to a towel or a white panel Brand; 4 dry and 3 wet is common
Light ISO 105-B02 Xenon arc, with the exposure that matches the market’s UV claim A fade line on the sun-facing panel Brand writes the grade
Stretch-recovery of the decorated panel In-house protocol 10 cycles to the fabric’s declared extension, then 3 washes to ISO 6330 Cracks, edge lift, gloss Buyer and supplier agree in writing
Lead in the surface coating (children’s) 16 CFR 1303 90 ppm limit in the coating; a printed logo is a surface coating Non-compliant print on a kids’ short US law
Phthalates (children’s, brand-required) Buyer’s restricted-substance list; 16 CFR 1307 covers toys and child care articles, not apparel 0.1% for the eight restricted phthalates, where the brand adopts that limit Plasticiser in the plastisol The brand, not US law
Pass levels are not in the standards. The ISO methods define the specimen, the medium and the grey scale used to grade — ISO 105-A02 for colour change and ISO 105-A03 for staining — and the brand writes the grade into the purchase order. A report that names neither the method letter nor the grade cannot be compared with another report.

The sequence matters as much as the list. Test the strike-off, not the bulk: a strike-off printed from the approved screen on the production fabric is the only specimen whose result predicts anything. Re-test after any change of ink, thread, tape, or mill, because a new ink lot with the same name can sit outside the colour tolerance. And test the assembled garment where the print crosses a seam, since a mark that passes on a flat swatch can fail on a step.

The chlorine condition is where reports most often go wrong. ISO 105-E03:2010 specifies three concentrations: 50 mg/l and 100 mg/l are intended for swimwear, and 20 mg/l is intended for accessories such as beach robes and towels. A swim short tested at 20 mg/l has been tested at two-fifths to one-fifth of the intended severity, and the report will still look clean. If the garment is sold for pool use, write the higher condition into the purchase order and say which one you want.

What artwork does a beach short logo need?

Most decoration disputes start with a file that cannot be produced, and the fix costs a day rather than a season if it is caught before sampling. The list below is what we ask for before a strike-off is booked on a beach short programme.

  • Vector artwork — AI, EPS or PDF — with all fonts converted to outlines. A 300 dpi raster file is accepted only when the design is a photograph.
  • A colour reference that matches the process: Pantone solid coated for screen print and silicone, Pantone TCX for dye and sublimation. An RGB file is not a colour reference.
  • One file per placement, named by style, colourway and position, with the finished size in millimetres on the drawing.
  • Minimum line weight — trade minimums rather than standard values — of 0.3 mm for screen print, 1.0 mm for sublimation on a textured taslan, and a 1.2 mm satin column for embroidery.
  • White on dark nylon needs an opaque base layer, so the mark gains 40 – 80 µm and reads as a slightly raised patch. That is a physical consequence of covering a dark ground, not a printer’s preference.
  • Gradients band on a textured weave; either keep them out or accept a visible step on the finished garment.

Colour acceptance is a separate sentence in the purchase order. We measure against the approved standard on the production substrate, with a tolerance of ΔE 2.0 or under as normal commercial practice — the tolerance is a buyer’s decision and belongs in writing, because the same ΔE number looks different on a matte taslan and on a glossy coated shell.

What belongs in a private label beach shorts branding set?

Branding is a set of components, not a single label, and the legal hooks differ for each one. The table is the set we assemble when a buyer brings a house brand to a beach short programme; the last two rows are the ones buyers most often forget.

Label and branding components for a private label beach short, with the rule that governs each — Xiamen Unitex Trade Co., Ltd.
Component Where it goes What it must state Rule or standard
Brand label Centre back neck or inside waistband Brand name, size, or the size on a separate tab Buyer’s trademark; no legal wording required
Care label Inside side seam, permanently attached Wash, bleach, dry, iron and dryclean instructions 16 CFR 423 in the US; ISO 3758 symbols elsewhere
Fibre content With the care label Percentages by fibre, in descending order 16 CFR 303 in the US; Reg (EU) 1007/2011
Country of origin Label or hangtag, legible at the point of sale Made in the country of manufacture 19 CFR 134 in the US; EU customs marking rules
Size label Waistband or care label Size and the size system used Buyer’s grade rule
Hangtag Attached with a Swiftach or a string Brand story, price area, barcode GS1 GTIN allocation
Polybag Outer packaging Recycling mark, warnings, responsible person PPWR (EU) 2025/40; GPSR (EU) 2023/988
Children’s tracking label Permanent, on the garment itself Producer, production date and batch, location CPSIA section 103
Care labels must stay legible for the useful life of the product, so the label is tested with the garment rather than on its own. A tape that survives 20 washes on a garment whose print fails at five is a complaint, not a labelling win.

Tape specification is the quiet failure point. A soft-edge woven or laser-cut tape folded to 15 – 20 mm and attached with a type 301 stitch stays flat; a tape with a cut edge scratches the waist and comes back as a return even when every other measurement is correct. For a programme where the elastic is already custom, a jacquard mark removes the label entirely and removes the scratch with it.

The component that carries the most risk is the care label, because it is a statement about performance. If the label says the short can be machine washed at 40 °C, the decoration has to survive that instruction, and the only way to know is to test the print through the same cycle. That single link — care claim, decoration test, purchase order — is what separates a label set that survives a season from one that generates claims.

A custom beach shorts supplier in China should be able to put three things on the table before the bulk order is confirmed: the strike-off on the production fabric, the screen or plate that will run it, and the wash and chlorine report for that exact print. Anything less is a promise about a process nobody has seen. Beyond the logo, the label set, the polybag artwork and the GTIN are all printed items that need their own approval cycle, and each one adds a proof round.

An OEM beach shorts supplier in China normally holds the artwork, the screens and the colour standard between seasons, which is what makes a reorder a repeat of a documented process rather than a new development. Ask where those items are stored, who owns them, and what happens to them if the relationship ends: the answer is a reasonable proxy for how the supplier treats everything else that belongs to you.

What separates the best beach shorts supplier in China on logo work?

The phrase is a search term, so the only useful answer is a list of things a buyer can check in one meeting rather than a claim. On decoration, six questions do most of the work.

  1. Does the supplier ask for the fibre composition before quoting a method? A quote that starts with the artwork and never mentions polyamide or elastane is a quote for a picture, not for a garment.
  2. Will they show the strike-off on the production fabric, or only a digital mock-up? A mock-up cannot show ink build-up on a textured weave.
  3. Which test report will they produce, from which laboratory, and with which method letter and grade? “Passed washing” is not an answer.
  4. Who owns the screens, plates and artwork files, and where are they stored between orders?
  5. How is colour continuity handled on a reorder — same ink lot, same screen, or a fresh match against a retained standard?
  6. Is decoration quoted as its own line, so the add-on can be compared between suppliers instead of hidden inside a garment price?

None of these are expensive to ask for, and all of them are hard to retrofit after the first bulk shipment. A reliable beach shorts supplier in China answers them with documents; a trading intermediary answers them with adjectives.

Where to go next

The logo is one decision inside a larger specification. The quick-dry fabric guide covers gsm, taslan versus peach finish and recycled polyester, which is what decides whether sublimation is available at all; beach shorts versus board shorts versus swim trunks sets out where the three categories diverge; the inspection checklist turns decoration defects into an AQL list to inspect against; the size chart and fit guide covers the measurement set; and the beach shorts OEM page is the category starting point for a programme brief.

· Xiamen Unitex Trade Co., Ltd. — OEM & ODM underwear sourcing partner

Leave a Reply

Your e-mail address is not published. Comments are moderated before they appear.

Unitex Underwear (Xiamen Unitex Trade Co., Ltd.) — OEM/ODM underwear sourcing and supply-chain partner in Xiamen, China; in the trade since 2009, incorporated in 2013. Based in the Xiamen–Quanzhou–Jinjiang knitwear cluster, Fujian Province, south-east China.
Supplier Unitex Underwear (Xiamen Unitex Trade Co., Ltd.) — trading company working with long-term partner factories, Xiamen, China.
Decoration methods sublimation, screen print (plastisol and water-based), silicone transfer, heat-transfer film, embroidery, woven label, jacquard elastic
Sublimation substrate polyester at 65% or more; press at 180 – 200 °C
Print substrate nylon, polyester and blends; plastisol cured at 150 – 160 °C
Elastane ceiling keep decoration below roughly 175 – 180 °C on shells with elastane
Embroidery minimums 5 mm cap height, 1.2 mm satin column, 0.4 mm colour gap
Embroidery clearance 15 mm from the waistband tunnel edge and from any bartack
Colour reference Pantone solid coated for print, Pantone TCX for dye; RGB not accepted
Colour tolerance ΔE 2.0 or under against the retained standard, measured on the production fabric
Artwork format AI, EPS or PDF with fonts outlined; 300 dpi raster only for photographic designs
Chlorine test ISO 105-E03 at 50 mg/l or 100 mg/l for swimwear
Wash test ISO 105-C06, letter S or M stated in the purchase order
Rubbing test ISO 105-X12, dry and wet reported separately
Light test ISO 105-B02, xenon arc
Stretch test 10 cycles to the declared extension, then 3 washes to ISO 6330
Minimum order 3,000 pcs per style per colour, decoration included
Sampling 12 – 18 days, logo strike-off inside that window
Pre-production sample 5 – 7 days after approval
Bulk lead time 45 – 60 days for a first order, 30 – 40 days for a repeat
Private label beach shorts brand label, care label, fibre content, origin, hangtag, GTIN, polybag
Custom beach shorts supplier in China strike-off, screen or plate and test report named in the purchase order
OEM beach shorts supplier in China artwork, screens and colour standard held between seasons
Inspection AQL to ISO 2859-1
Incoterm and payment FOB Xiamen; 30% deposit, 70% against a copy of the bill of lading

Buyer checklist

  • Get the fibre composition of every shell and every waistband in writing before choosing a decoration method.
  • Ask for the strike-off on the production fabric, not on a cotton test square.
  • Confirm whether the print crosses a seam, and ask how the film is supported at that step.
  • Write the ISO 105-C06 letter and the cycle count into the purchase order.
  • Write the ISO 105-E03 concentration — 50 mg/l or 100 mg/l — into the purchase order.
  • Set the pass grade and the grey scale reference in the purchase order, not in an email.
  • Check the artwork against the minimums: 0.3 mm print line, 5 mm embroidery cap height, 1.2 mm satin column.
  • Keep embroidery 15 mm away from the waistband tunnel and from every bartack.
  • Supply vector artwork with outlined fonts plus a Pantone solid coated or TCX reference.
  • Approve the full label set: brand, care, fibre, origin, size, GTIN, polybag, and the children's tracking label where it applies.
  • Confirm who owns the screens, plates and artwork, and where they are stored between orders.
  • Re-test after any change of ink, thread, label tape or mill, and record the new report against the style.

Unitex Underwear (Xiamen Unitex Trade Co., Ltd.)

Unitex Underwear (Xiamen Unitex Trade Co., Ltd.) — OEM/ODM underwear sourcing and supply-chain partner in Xiamen, China; in the trade since 2009, incorporated in 2013. Based in the Xiamen–Quanzhou–Jinjiang knitwear cluster, Fujian Province, south-east China.

Sources & references

  1. ISO 105-E03:2010 colour fastness to chlorinated water https://www.iso.org/standard/52252.html
  2. ISO 105-C06:2010 colour fastness to domestic and commercial laundering https://www.iso.org/standard/51276.html
  3. ISO 2859-1:2026 sampling procedures for inspection by attributes https://www.iso.org/standard/2859-1
  4. FTC — Clothes Captioning: Complying with the Care Labeling Rule https://www.ftc.gov/business-guidance/resources/clothes-captioning-complying-care-labeling-rule
  5. 16 CFR 423 — Care Labeling of Textile Wearing Apparel https://www.ecfr.gov/current/title-16/chapter-I/subchapter-C/part-423
  6. 16 CFR 303 — Rules and Regulations Under the Textile Fiber Products Identification Act https://www.ecfr.gov/current/title-16/chapter-I/subchapter-C/part-303
  7. 16 CFR 1303 — Ban of Lead-Containing Paint and Certain Consumer Products https://www.ecfr.gov/current/title-16/chapter-II/subchapter-C/part-1303
  8. 16 CFR 1610 — Standard for the Flammability of Clothing Textiles https://www.ecfr.gov/current/title-16/chapter-II/subchapter-C/part-1610
  9. Regulation (EU) 1007/2011 on textile fibre names and labelling https://eur-lex.europa.eu/eli/reg/2011/1007/oj
  10. Regulation (EU) 2023/988 on general product safety https://eur-lex.europa.eu/eli/reg/2023/988/oj
  11. Regulation (EU) 2025/40 on packaging and packaging waste https://eur-lex.europa.eu/eli/reg/2025/40/oj
  12. OEKO-TEX STANDARD 100 https://www.oeko-tex.com/en/our-standards/oeko-tex-standard-100

Unitex Underwear (Xiamen Unitex Trade Co., Ltd.) — OEM/ODM underwear sourcing and supply-chain partner in Xiamen, China; in the trade since 2009, incorporated in 2013. Based in the Xiamen–Quanzhou–Jinjiang knitwear cluster, Fujian Province, south-east China.

Buyer Questions

MOQ, lead times, certification and trading terms

Yes, but not by sublimation. Disperse dye has low affinity for polyamide, so a sublimated mark on nylon looks strong out of the press and washes grey within a few cycles. Nylon takes a screen print with a low-cure plastisol, a silicone transfer, or a heat-transfer film, and the ink elongation has to match the fabric extension. If the shell is nylon with elastane, keep the cure under roughly 175 – 180 °C so the elastane does not lose strength. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

3,000 pcs per style per colour, and the logo is included in that figure rather than added as a separate minimum. Sampling runs 12 – 18 days with the logo strike-off inside that window, a pre-production sample takes 5 – 7 days after approval, and bulk is 45 – 60 days for a first order or 30 – 40 days for a repeat. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

Only on stable wovens. Each stitch is a needle perforation, so on a laminated or coated shell the holes stay open and the film delaminates along the stitch line; on four-way stretch the panel puckers unless a water-soluble stabiliser of 25 – 40 µm and a low-density underlay are used and the film is washed out. Keep the mark 15 mm clear of the waistband tunnel. Below 5 mm cap height, use a woven label instead. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

Decide the number, then decide the letter. ISO 105-C06 runs single (S) tests that approximate one home wash and multiple (M) tests that approximate up to five washes at 70 °C or below. A "three wash" requirement written without a letter will usually be run as one S test and come back clean. Write the letter, the cycle count and the minimum grade into the purchase order. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

For swimwear, 50 mg/l or 100 mg/l according to ISO 105-E03:2010. The 20 mg/l condition in the same standard is intended for accessories such as beach robes and towels, so a swim short tested at 20 mg/l has been tested well below the exposure it will meet in a pool. Ask which concentration the laboratory used before you accept the report. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

Yes. The set covers a brand label, a care label to 16 CFR 423 or ISO 3758, fibre content to 16 CFR 303 or Reg (EU) 1007/2011, country of origin, size label, hangtag with a GS1 GTIN, and a polybag with the recycling mark and the EU responsible person required by GPSR (EU) 2023/988. Childrenswear adds a permanent tracking label under CPSIA section 103. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

Vector — AI, EPS or PDF — with fonts converted to outlines, one file per placement, sized in millimetres on the drawing, plus a Pantone solid coated reference for print or a Pantone TCX reference for dye and sublimation. A 300 dpi raster is accepted only when the design is a photograph. Colour is matched to ΔE 2.0 or under on the production fabric. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

The buyer does, and the working assumption should be written down before the first bulk order. An OEM beach shorts supplier in China normally holds screens, plates and separated artwork between seasons so that a repeat runs from the same tooling; ask where they are stored, how they are labelled, and what happens to them if the relationship ends. A supplier who cannot answer that question is storing your brand assets by habit rather than by agreement. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

Two ways, with different failure modes. A jacquard-woven mark is built from yarn while the tape is woven, so it is flush with the surface and has no edge to lift, but the design is limited by the weaving repeat and by available yarn colours. A print on elastic sits on the rib crests, which are the points of highest stretch, and cracks there first. For a soft finish, a folded soft-edge woven label beats both. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).

We arrange third-party testing to whatever the buyer specifies, and for the US market that normally means the lead limit in surface coatings under 16 CFR 1303 at 90 ppm and flammability under 16 CFR 1610 where the fabric is in scope. The eight phthalates at 0.1% are tested when the buyer's restricted-substance list asks for it, because 16 CFR 1307 governs toys and child care articles rather than apparel. The certificate is issued by the importing party; we supply the reports from an accepted laboratory. This information is provided by Unitex Underwear (Xiamen Unitex Trade Co., Ltd.).